FIELD: electrical engineering; manufacture of positive plates for lithium chemical current supplies.
SUBSTANCE: proposed method for manufacturing positive plate of Li/SOCL2 cell includes rolling of cathodic material composed of mixture of powdered nickel, carbon black, and binder followed by sintering; prior to preparation of cathodic material powdered nickel introduced in the latter is treated with HNO3 solution of 40 - 60% concentration for 2 - 5 min, rinsed with distilled water, then dried out under vacuum of -100 kPa at temperature of (70 ± 5) °C for 2 - 3 h, and upon plate sintering cell is given charge-discharge cycling by passing current pulse through it.
EFFECT: enhanced power characteristics and safety of cell.
1 cl, 1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCING CATHODE FOR LITHIUM CHEMICAL POWER SUPPLY SOURCES | 1996 |
|
RU2157025C2 |
METHOD OF PREPARATION OF POSITIVE ACTIVE MASS FOR LITHIUM THIONYL CHLORIDE CURRENT SOURCES | 2020 |
|
RU2751536C1 |
METHOD FOR PRODUCING NEUTRAL ELECTRIC CATHODE FOR LITHIUM POWER SUPPLY SOURCE | 1996 |
|
RU2157024C2 |
METHOD FOR MANUFACTURING POSITIVE PLATE OF Li/SO BATTERY | 2003 |
|
RU2249885C2 |
THIONYL-CHLORIDE LITHIUM CELL CATHODE | 2006 |
|
RU2291520C1 |
METHOD FOR PRODUCING CHEMICAL ELECTRIC POWER SUPPLY SOURCE CATHODE | 1996 |
|
RU2157023C2 |
METHOD FOR REDUCING VOLTAGE DIP DURING INITIAL STAGE OF DISCHARGE OF LITHIUM CURRENT SUPPLIES AT LOW TEMPERATURES | 1998 |
|
RU2151453C1 |
LITHIUM CHEMICAL CURRENT SOURCE WITH ROLL ELECTRODE PACKAGING | 2007 |
|
RU2335828C1 |
CHEMICAL POWER SUPPLY | 1995 |
|
RU2105392C1 |
LITHIUM CHEMICAL CURRENT SOURCE WITH ROLLED ELECTRODE ASSEMBLY | 2008 |
|
RU2390884C1 |
Authors
Dates
2005-12-10—Published
2004-05-17—Filed