FIELD: rechargeable lithium cells. SUBSTANCE: thermal stability of cell is ensured due to exposure of charged cell to temperature ranging between 20 and 75 c for 1 h to 2 months, best for 1 h to 72 h. EFFECT: improved thermal stability of cell. 10 cl, 2 tbl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
IMPROVED METHOD OF PREPARING LITHIUM DOPE SPINEL OF LITHIUM-MANGANESES OXIDE | 1996 |
|
RU2152355C1 |
ELECTROCHEMICAL DEVICE INCORPORATING ALIPHATIC NITRILE JOINT | 2005 |
|
RU2308792C1 |
METHOD OF PREPARING LITHIUM-MANGANESE OXIDE LiMnO WITH SPINEL STRUCTURE (VARIETIES) AND SECONDARY RECHARGEABLE BATTERY | 1997 |
|
RU2165390C2 |
METHOD OF PREPARING GAMMA-MANGANESE DIOXIDE, HYBRID MATERIAL CONTAINING GAMMA-MANGANESE DIOXIDE, AND ELECTROLYTIC CELL | 1993 |
|
RU2118292C1 |
RECHARGEABLE POSITIVE PLATE | 1995 |
|
RU2143768C1 |
SYSTEM OF STABLE HIGH-TEMPERATURE SECONDARY BATTERY AND METHOD RELATED THERETO | 2018 |
|
RU2740794C1 |
ELECTROCHEMICAL CURRENT SUPPLY AND ELECTRONIC DEVICE INCORPORATING MOISTURE-SENSING COMPONENT | 1992 |
|
RU2119702C1 |
SECONDARY ELEMENT USING SULFUR-ORGANIC/METAL MATERIALS OF CHARGE TRANSFER AS POSITIVE ELECTRODE | 1995 |
|
RU2133526C1 |
TESTER FOR BATTERY | 1996 |
|
RU2182712C2 |
CHEMICAL SOURCE ANODE | 1995 |
|
RU2096866C1 |
Authors
Dates
2000-09-20—Published
1996-06-05—Filed