FIELD: leather industry. SUBSTANCE: raw material is washed, limed with 3-5% lime of the weight of raw material for 10-12 h, de-ashed with 2-3% of ammonium sulfate, tanned with 8-12% of tanning agent for 3-4 h, dyed, and greased. EFFECT: improved strength characteristics of leather. 1 tbl, 5 ex