FIELD: manufacture of titanium alloy structure; sheet stamping and die forging; heat treatment of titanium alloys. SUBSTANCE: proposed method includes cleaning blanks, machining degreasing in acetone or in cleaning fluids dehydration in commercial alcohol, heating blanks in heat-treating furnace at temperature of 250 to 280 C for 1.5 to 2.0 hours for forming dense oxide film on surface followed by applying the protective coat and drying it. EFFECT: improved technological and protective properties of coats; reduced content of gas admixtures in surface layer of finished articles. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PREPARING FOR WELDING EDGES OF SHEET BLANKS OF TITANIUM ALLOYS | 2001 |
|
RU2196032C1 |
METHOD OF TITANIUM ALLOYS BLANKS PREPARATION FOR WELDING | 1992 |
|
RU2076029C1 |
METHOD OF ONE-PASS ARC WELDING OF TITANIUM AND TITANIUM ALLOY ARTICLES OF THICKNESS FROM 10 MM AND GREATER OVER GAS-SATURATED EDGES | 1999 |
|
RU2156680C1 |
TITANIUM ALLOY PIPE EXPANDING DIE | 1996 |
|
RU2104815C1 |
DEVICE FOR ELECTROTHERMAL TREATMENT OF SHEET BAR | 1999 |
|
RU2170771C2 |
METHOD OF HARDENING TITANIUM ALLOYS (VERSIONS) | 2000 |
|
RU2202629C2 |
MEDIUM FOR COMPLEX SATURATION OF METAL SURFACE | 1998 |
|
RU2133298C1 |
FACILITY TO TREAT MAGNESIUM ALLOYS BY GASES IN PROCESS OF FLUX-FREE PREPARATION | 2000 |
|
RU2173722C1 |
DIE SET FOR SHAPING TUBULAR BLANKS | 1996 |
|
RU2094155C1 |
METHOD OF HARDENING OF ARTICLES FROM STEELS AND ALLOYS | 2000 |
|
RU2186859C2 |
Authors
Dates
2001-11-27—Published
1999-11-16—Filed