FIELD: antifriction materials. SUBSTANCE: polytetrafluoroethylene-based composition contains 1.0 to 2.0 wt % synthetic alumina (brand mark 124127) activated in double-motion paddle mill during 2 min. Composition can be used for manufacturing sealing members for couples performing rotational and reciprocal movements and for friction units. EFFECT: increased wear resistance, deformation and strength properties, and carrying capacity of material. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
TRIBOTECHNICAL-DESTINATION POLYMER COMPOSITION | 2000 |
|
RU2177963C1 |
ANTIFRICTION POLYMER COMPOSITION WITH SEALING CAPABILITY | 1994 |
|
RU2114874C1 |
ANTIFRICTION POLYMER COMPOSITION | 2004 |
|
RU2296139C2 |
METHOD OF PREPARING ANTIFRICTION COMPOSITION | 1997 |
|
RU2178801C2 |
ANTIWEAR RESIN COMPOSITION | 2005 |
|
RU2281960C1 |
ANTI-FRICTION POLYMER COMPOSITION | 2007 |
|
RU2329279C1 |
COMPOSITE DIAMOND-CONTAINING POLYMERIC MATERIAL FOR ABRASIVE TOOLS | 1999 |
|
RU2164522C1 |
POLYMER COMPOSITION FOR TRIBOTECHNICAL PURPOSES | 2011 |
|
RU2484107C1 |
ANTI-FRICTION POLYMER COMPOSITION | 2010 |
|
RU2460742C2 |
POLYMER MATERIAL FOR TRIBOTECHNICAL PURPOSES | 2017 |
|
RU2664129C1 |
Authors
Dates
2002-01-10—Published
2000-04-19—Filed