FIELD: manufacture of building materials. SUBSTANCE: proposed composition includes cement, sand, expanded granules of foam polystyrene and water; it also contains complex additive consisting of 0.015 wt-% of sulfate soap and 0.15 wt-% of commercial lignoulfonate in terms of mass of composition at the following ratio of components, mass-%: cement, 50 to 51; sand, 30 to 31; expanded granules of foam polystyrene, 2.1 to 2.2; above-mentioned additive, 0.165 and water being remainder. EFFECT: enhanced adhesion of granules to binder; plasticization of concrete mix; reduced density of finished articles. 3 tbl
Title | Year | Author | Number |
---|---|---|---|
COMPOSITION FOR MANUFACTURE OF LIGHT-CONCRETE PRODUCTS | 2000 |
|
RU2181707C2 |
POLYSTYRENE CONCRETE | 2023 |
|
RU2819771C1 |
AGGLUTINANT SAND FOR HEAT-INSULATING MATERIAL PRODUCTION | 2007 |
|
RU2341495C1 |
RAW MIX FOR PRODUCING LIGHT CONCRETE | 0 |
|
SU1636386A1 |
METHOD OF MANUFACTURING HEAT-INSULATION PRODUCTS | 2003 |
|
RU2254310C1 |
RAW MIX FOR FIRE RESISTANT STRUCTURAL-HEAT INSULATION CONCRETE | 2007 |
|
RU2356865C2 |
AERATED LIGHT CONCRETE | 2005 |
|
RU2288904C1 |
METHOD OF PRODUCING SLAG-CONCRETE MIX | 0 |
|
SU1470712A1 |
RAW MIXTURE FOR PRODUCING LIGHTWEIGHT CONCRETE | 0 |
|
SU1296542A1 |
METHOD OF PREPARING HIGH-MODULUS LIQUID GLASS | 2000 |
|
RU2171221C1 |
Authors
Dates
2002-05-10—Published
2000-03-20—Filed