FIELD: polymers. SUBSTANCE: invention relates to technology of preparing compositions from aramide fibers and polymer used for reinforcement of elastomeric and thermoplastic polymeric materials. Aramide fibers are wetted to moisture content 20-85 wt.% and added their into extruder with supplied heat at constant rate followed by effect by shearing force on fibers. Then polymer is added continuously, components are stirred and composition is removed from extruder. Invention provides preparing the HOMOGENIZE composition in continuous regimen. EFFECT: improved method of composition preparing. 16 cl, 1 dwg, 3 tbl, 5 ex
Authors
Dates
2002-05-20—Published
1998-08-11—Filed