FIELD: electrical engineering. SUBSTANCE: electrode has composite lithium base oxide as active material meeting 1.5≤Sa/Sc≤10 relation, where Sa is specific surface area measured by BET method; r is particle diameter; f(r) is particle distribution; d is particle density of mentioned composite lithium base oxide; Sc is quantity found from formula . EFFECT: improved capacity and discharge characteristics. 3 cl, 2 dwg, 2 tbl, 3 ex
Title | Year | Author | Number |
---|---|---|---|
ELECTRODE FOR STORAGE BATTERY WITH NONAQUEOUS ELECTROLYTE | 1998 |
|
RU2183369C2 |
PLATE MANUFACTURING PROCESS FOR STORAGE BATTERY USING NONAQUEOUS ELECTROLYTE | 1998 |
|
RU2183886C2 |
ACCUMULATOR BATTERY WITH NON-AQUEOUS ELECTROLYTE | 2013 |
|
RU2569670C1 |
ACCUMULATOR BATTERY WITH NON-AQUEOUS ELECTROLYTE | 2012 |
|
RU2574592C2 |
ACTIVE MATERIAL OF POSITIVE ELECTRODE FOR LITHIUM-ION SECONDARY BATTERY | 2012 |
|
RU2540072C1 |
ELEMENT FOR MANUFACTURE OF SECONDARY BATTERIES | 1992 |
|
RU2099821C1 |
COMPOSITIONS OF POSITIVE ELECTRODE FOR SECONDARY BATTERY WITH NONAQUEOUS ELECTROLYTE | 2013 |
|
RU2618229C2 |
ELECTRODE AND ELECTRIC ACCUMULATING DEVICE FOR LEAD-ACID SYSTEM | 2011 |
|
RU2585240C2 |
ACTIVE MATERIAL OF POSITIVE ELECTRODE FOR ELECTRIC DEVICE, POSITIVE ELECTRODE FOR ELECTRIC DEVICE AND ELECTRIC DEVICE | 2012 |
|
RU2556239C1 |
LITHIUM CELL IMPROVEMENT TECHNIQUE | 1996 |
|
RU2156523C2 |
Authors
Dates
2002-06-10—Published
1998-05-27—Filed