FIELD: metallurgy; preparation of compounds for modification of cast- iron; manufacture of high-strength parts. SUBSTANCE: mixture contains the following components, mas.%: ultradispersed powder of metal oxide of groups IV-VIII, 60-70; aluminum powder, 20-25; and carbon-containing material, 10-15. EFFECT: increase of tensile strength by 20-25% without use of expensive magnesium bases; reduced power requirements; reduced consumption of modifying agent. 3 cl, 1 tbl, 1 ex
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD OF MODIFICATION OF CAST IRON | 2003 |
|
RU2254377C1 |
| MIXTURE FOR CAST IRON TREATMENT | 2002 |
|
RU2213145C1 |
| METHOD FOR MAKING HIGH-STRENGTH IRON CASTINGS | 2001 |
|
RU2200646C2 |
| MIXTURE FOR TREATMENT OF CAST IRON | 2001 |
|
RU2186121C1 |
| CAST IRON AND SILUMIN MODIFYING METHOD | 2010 |
|
RU2439166C2 |
| MODIFICATION METHOD OF ALUMINIUM AND ALUMINIUM-SILICONE ALLOYS (SILUMINS) BY CARBON | 2013 |
|
RU2538850C2 |
| METHOD OF MODIFYING GREY IRON | 2002 |
|
RU2219246C2 |
| METHOD OF PRODUCING WEAR-RESISTANT WHITE IRON | 2009 |
|
RU2412780C1 |
| METHOD FOR MODIFICATION OF CAST IRON | 2015 |
|
RU2588965C1 |
| CAST IRON TREATMENT MODIFIER | 1993 |
|
RU2069703C1 |
Authors
Dates
2002-12-27—Published
2001-09-13—Filed