FIELD: mechanical engineering. SUBSTANCE: modified wood comprises compressed wood, ceresine, polyethylene, polyethylsiloxane and aerosil, said components being used in predetermined ratio. Modified wood is used for manufacture of friction parts operating under increased temperature conditions. EFFECT: increased wear-resistance and prolonged service life. 2 tbl, 5 ex
Title | Year | Author | Number |
---|---|---|---|
ANTIFRICTION COMPRESSED WOOD FOR MAKING PARTS OF FRICTION | 2012 |
|
RU2491162C1 |
ANTIFRICTION COMPRESSED WOOD | 2002 |
|
RU2221821C1 |
METHOD FOR PRODUCTION OF PLATES OF SUNFLOWER HUSK | 2000 |
|
RU2196045C2 |
PARQUET BLANK MANUFACTURE METHOD | 1997 |
|
RU2118928C1 |
METHOD FOR MANUFACTURE OF WOOD PARTICLE BOARDS | 2000 |
|
RU2176186C1 |
ANTIFRICTION COMPRESSED WOOD | 2002 |
|
RU2235635C2 |
FRICTION UNIT WITH RADIAL-AXIAL BEARING MADE OF MODIFIED WOOD | 2000 |
|
RU2222724C2 |
METHOD FOR MANUFACTURE OF PLATES FROM SUNFLOWER HUSK | 2004 |
|
RU2252866C1 |
UNIT OF FRICTION WITH BEARING FROM PRESSED WOOD | 2011 |
|
RU2462626C1 |
METHOD AND DEVICE FOR PRODUCTION OF MODIFIED WOOD | 1999 |
|
RU2151691C1 |
Authors
Dates
2003-01-27—Published
2000-12-13—Filed