FIELD: mechanical engineering; application of coats by gas thermal methods. SUBSTANCE: proposed method includes preheating of parts to 400-500 C, fusion in air and subsequent heat treatment performed at two stages; first parts are kept at temperature which is below temperature of beginning of martensitic transformation by 50-150 C for 1-2 h, after which temperature is raised at rate of 8-12 deg./min till magnitude corresponding to maximum rate of process of austenitic disintegration and parts are kept at this temperature for 2-3 h; then, they are cooled to room temperature at rate of 1-2 deg./min. EFFECT: reduced cracking; increased hardness of coat. 1 tbl, 1 ex
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD OF TREATMENT OF FLAME-SPRAYED COATS OF SELF-FLUXING ALLOYS | 0 |
|
SU1713975A1 |
| METHOD OF APPLYING COATINGS | 0 |
|
SU1553569A1 |
| COMPOSITION FOR HARD FACING BY GAS-THERMIC SPRAYING | 0 |
|
SU1633013A1 |
| WORN SURFACE OF STEEL PARTS RESTORATION METHOD | 2005 |
|
RU2299115C1 |
| RESTORATION METHOD OF WORN-OUT SURFACES OF STEEL PARTS | 2013 |
|
RU2532738C1 |
| METHOD OF FORMING COATINGS FROM SELF-FLUXING POWDERED MATERIALS ON IRON-CARBON ALLOY ARTICLES | 1997 |
|
RU2112815C1 |
| PROCEDURE FOR PRODUCTION OF GAS-THERMAL COATING OUT OF POWDER WIRES | 2008 |
|
RU2394936C2 |
| METHOD OF PRODUCING WEAR-RESISTANT COATINGS | 0 |
|
SU1541305A1 |
| METHOD FOR MANUFACTURING PARTS WITH HARDENED WORKING SURFACE | 1996 |
|
RU2109843C1 |
| METHOD OF PLASMA APPLICATION OF COATS | 2000 |
|
RU2198239C2 |
Authors
Dates
2003-03-27—Published
2000-11-20—Filed