FIELD: electrical engineering; lighting lamp manufacture. SUBSTANCE: proportion of phosphor mixture ingredients is as follows, mass percent: powdered phosphor, 65.0-84.5; binder (boron oxide), 1.0-4.0; filler, the rest. At least 60% of powdered phosphor should have grain size up to 20 mcm. Quartz powder, milled sapphire powder, or crushed polycrystalline aluminum oxide may be used as filler. Ingredients are mixed up for 15-20 minutes, dried out at 100±5 C for 2.5-3.5 h, and cooled down. EFFECT: reduced cost of lamp manufacture; enhanced productivity of coating process. 1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
PHOTOLUMINOPHOR MIXTURE FOR PRODUCTION OF PHOTOLUMINESCENT FILM OF WHITE LEDS | 2014 |
|
RU2565670C1 |
GASEOUS DISCHARGE LAMP FOR FLUORIMETRIC ANALYSIS | 1993 |
|
RU2077088C1 |
METHOD FOR APPLYING POWDER MIXTURE TO GLASS BULBS OF OPTICAL-RADIATION POWER SUPPLIES | 2002 |
|
RU2233508C2 |
LUMINOPHOR SUSPENSION FOR GAS-DISCHARGE SOURCE OF LIGHT | 1994 |
|
RU2064711C1 |
LUMINOPHOR MIXTURE AND FLUORESCENT LAMP CONTAINING IT | 2010 |
|
RU2556105C2 |
PHOSPHOR SUSPENSION FOR GAS-DISCHARGE LIGHT SOURCES | 1993 |
|
RU2040069C1 |
LUMINOPHORE SUSPENSION FOR FLUORESCENT LIGHT SOURCES | 1994 |
|
RU2079536C1 |
GAS TUBE | 2008 |
|
RU2376671C1 |
PHOSPHOR SUSPENSION FOR GAS-DISCHARGE LIGHT SOURCES | 1993 |
|
RU2040070C1 |
LUMINESCENT SOLID SUSPENSION | 1990 |
|
SU1748431A1 |
Authors
Dates
2003-03-27—Published
2000-12-13—Filed