FIELD: refractory materials. SUBSTANCE: invention relates to technology for preparing refractory articles used in high-temperature units. Charge for preparing refractory articles comprises the following components, wt.-%: kaolin, 26-28; refractory clay, 23-25; quartz sand, 38.4-42; alumina production waste, 6-10 and 0.6-0.8% of Cr2O3 additionally. Invention provides decrease of roasting temperature and high working temperature. EFFECT: improved properties of charge. 2 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| NEPHRITED FUSIBLE GLAZE | 2001 |
|
RU2206529C1 |
| CERAMIC BODY | 1999 |
|
RU2174500C2 |
| GLASS FOR MANUFACTURING FOAMED MATERIAL | 2002 |
|
RU2235694C2 |
| COMPOSITION FOR PREPARING RADIATION-PROTECTION MATERIAL (OPTIONS) | 2003 |
|
RU2263983C2 |
| METHOD FOR PROCESSING LOW-QUALITY ALKALINE ALUMOSILICATE RAW | 2001 |
|
RU2213057C2 |
| METHOD FOR PROCESSING DISTHENE-ANDALUSITE-SILLIMANITE CONCENTRATE | 2002 |
|
RU2223914C2 |
| GLAZE | 1991 |
|
RU2024446C1 |
| PORCELAIN COMPOUND | 1997 |
|
RU2139265C1 |
| CERAMIC BODY FOR MANUFACTURING INSULATORS | 1999 |
|
RU2140405C1 |
| RAW MIXTURE FOR PELLETIZED GLASS FOAM | 2003 |
|
RU2243174C1 |
Authors
Dates
2003-07-10—Published
2001-10-26—Filed