FIELD: manufacture of building materials. SUBSTANCE: raw meal contains 77.5-80% of Cambrian lumpy clay from deposit Tsekalovsky, 12-15% of mortar sand with fineness modulus 2-2.5, and 5-95% of combustible fibrous additive (cellolignin) with moisture content 4-6% and dispersity 0.5-1 mm. EFFECT: reduced specific weight and heat conductivity of brick at the same or higher compaction strength. 1 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| RAW MIX FOR MANUFACTURING CERAMIC BRICKS | 2005 |
|
RU2287504C1 |
| CERAMIC MIX FOR CONSTRUCTION BRICK MANUFACTURE | 2015 |
|
RU2596027C1 |
| RAW MATERIAL MIXTURE FOR MANUFACTURING CERAMIC BRICKS | 2015 |
|
RU2620677C1 |
| RAW MIX FOR CERAMIC BRICK MANUFACTURE | 2014 |
|
RU2567585C1 |
| RAW MATERIAL MIXTURE FOR MANUFACTURING OF POROUS BUILDING MATERIALS | 1997 |
|
RU2107050C1 |
| CERAMIC MIXTURE FOR MAKING CONSTRUCTION ARTICLES | 2018 |
|
RU2698369C1 |
| MANUFACTURING METHOD OF HEAT-INSULATING CERAMIC MATERIAL | 2007 |
|
RU2355665C1 |
| CERAMIC BRICK, STONE, AND METHOD OF FABRICATING CERAMIC BRICK AND STONE | 1997 |
|
RU2120923C1 |
| CERAMIC MASS | 1994 |
|
RU2081088C1 |
| CERAMIC MASS FOR CLARIFIED FINISHING BUILDING BRICKS | 2021 |
|
RU2787506C1 |
Authors
Dates
2004-05-27—Published
2002-04-29—Filed