FIELD: refractory materials. SUBSTANCE: invention provides charge for manufacturing refractory materials for use as lining for high-temperature assemblies such as smelting furnaces, ladles, crucibles for smelting, treatment, and transportation of different metals. Charge contains 45-55% baddeleyite concentrate/brucite mixture (85:15) and 45-55% kaolin and particle size of components is 8-9 mcm. EFFECT: improved strength and crack resistance characteristics in materials obtained from claimed raw material and considerably lowered expenses. 1 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD OF PREPARING COMPOSITE POWDERY MATERIAL OF ZIRCONIUM-CONTAINING MINERAL STOCK | 1999 |
|
RU2167128C2 |
| PROCESS OF RECEIVING COMPOSITION CERAMIC POWDER ON THE BASIS OF SILICON NITRIDE AND ZIRCONIUM OXIDE AND CHARGE FOR ITS IMPLEMENTATION | 2007 |
|
RU2351435C1 |
| CARBON-CONTAINING REFRACTORY MATERIAL | 1998 |
|
RU2151124C1 |
| METHOD TO PRODUCE COMPOSITION MATERIAL BASED ON TUNGSTEN-COPPER PSEUDOALLOY | 1993 |
|
RU2043867C1 |
| METHOD FOR PRODUCTION OF CERAMIC MATERIAL BASED ON ZIRCONIUM DIBORIDE | 1992 |
|
RU2053209C1 |
| MIXTURE FOR PRODUCTION OF MELT REFRACTORY MATERIALS | 1992 |
|
RU2081094C1 |
| METHOD OF PREPARING MODIFYING ADDITIVE | 1998 |
|
RU2168484C2 |
| METHOD FOR PRODUCTION OF ALUMINOSILICATE PROPANT AND COMPOSITION THEREOF | 2009 |
|
RU2392251C1 |
| METHOD OF MAKING ALUMINOSILICATE PROPPANT AND COMPOSITION FOR MAKING SAID PROPPANT | 2009 |
|
RU2389710C1 |
| CHARGE FOR REFRACTORY ARTICLE MAKING | 1998 |
|
RU2132312C1 |
Authors
Dates
2004-05-27—Published
2002-06-10—Filed