FIELD: low-voltage switching devices. SUBSTANCE: laminated electric contact has silver-containing effective layer and copper or copper alloy auxiliary layer; open surface of auxiliary layer is embossed in the form of semi-spheres. Embossed semi-sphere diameter ranges between 0.5 and 1.0 mm. There are three such embossed semi-spheres. Introduction of embossed semi-spheres makes it possible to attain high current density at contacting points and complete fusion of semi-sphere material. EFFECT: enhanced reliability of contact welding to contact holder. 1 cl, 3 dwg, 2 ex
Title | Year | Author | Number |
---|---|---|---|
LAMINATED ELECTRIC CONTACT | 2002 |
|
RU2229753C1 |
LAMINATED ELECTRIC CONTACT | 2002 |
|
RU2221299C1 |
WIRE OF SILVER-CONTAINING MATERIAL FOR PRODUCING ELECTRIC CONTACTS | 2002 |
|
RU2219608C1 |
METHOD OF PREPARATION OF CHARGE FOR LAMELLAR ELECTRIC CONTACT | 2002 |
|
RU2223843C1 |
LAMINATED ELECTRIC CONTACT | 2002 |
|
RU2228557C1 |
LAMINATED ELECTRIC CONTACT | 1991 |
|
RU2033653C1 |
CERMET BIMETALLIC ELECTRIC CONTACT | 0 |
|
SU1001207A1 |
MIXTURE FOR PRECOAT OF SILVER-CONTAINING BIMETALLIC ELECTRIC CONTACT BASED ON COPPER POWDER | 1989 |
|
SU1598748A1 |
PROCESS FOR MANUFACTURING ELECTRIC CONTACT | 0 |
|
SU1108522A1 |
BIMETALLIC CEMENT CONTACT | 0 |
|
SU1064335A1 |
Authors
Dates
2004-05-27—Published
2002-09-11—Filed