FIELD: building materials.
SUBSTANCE: invention can be used in making building blocks. Clay-phosphate material comprising clay, iron-containing waste in metallurgical manufacturing based on ferrous oxide Fe (II) with residue 5-7% on sieve № 008, ortho-phosphoric acid with density 1.24-1.25 g/cm3, Cambrian sky-blue clay and, additionally, open-hearth dust containing Fe (III) and Zn (II) oxides with residue 2-5% on sieve № 008 in the following ratio of components, wt.-%: Cambrian sky-blue clay, 56-57; indicated waste, 9-11; indicated open-hearth dust, 15-16; ortho-phosphoric acid with density 1.24-1.25 g/cm3, the balance. Invention provides enhancing resistance to cold of phosphate material.
EFFECT: valuable properties of material.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
CLAY-PHOSPHATE MATERIAL | 2008 |
|
RU2378221C1 |
CLAY-PHOSPHATE MATERIAL | 2004 |
|
RU2278843C1 |
CLAY-PHOSPHATE MATERIAL | 2006 |
|
RU2306293C1 |
CLAY-PHOSPHATE MATERIAL | 2009 |
|
RU2403220C1 |
CLAY-PHOSPHATE MATERIAL | 2004 |
|
RU2278844C1 |
CLAY-PHOSPHATE MATERIAL | 2012 |
|
RU2485071C1 |
CLAY-PHOSPHATE MATERIAL | 2004 |
|
RU2254307C1 |
CLAY-PHOSPHATE MATERIAL | 2007 |
|
RU2360888C1 |
CLAY-PHOSPHATE MATERIAL | 2008 |
|
RU2378220C1 |
CLAY-PHOSPHATE MATERIAL | 2004 |
|
RU2257359C1 |
Authors
Dates
2004-07-10—Published
2002-11-28—Filed