FIELD: oil and gas production.
SUBSTANCE: mortar contains Portland cement and tempering fluid prepared by adding water to additive prepared by dissolving aluminosilicate, in particular nepheline concentrate, in 3-20% hydrochloric acid solution, amount of additive constituting 3 to 30% of the weight Portland cement and water/cement ratio being 0.5-1.0. Thus obtained nepheline sol is treated with 5-10% lime milk until pH of mortar achieved 4.5-5.5.
EFFECT: reduced density of grouting mortar, increased strength of cement stone, and improved workability of additive.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
LIGHT-WEIGHT GROUTING MORTAR | 2000 |
|
RU2184211C2 |
METHOD FOR PRODUCING BINDER | 2023 |
|
RU2811516C1 |
METHOD FOR INDUSTRIAL SEWAGE TREATMENT | 1993 |
|
RU2049735C1 |
ACID-SOLUBLE BACKFILL COMPOSITION | 2010 |
|
RU2452757C1 |
BINDING AGENT | 1997 |
|
RU2125545C1 |
LIGHT GROUTING MORTAR | 1999 |
|
RU2151271C1 |
LIGHTENED GROUTING CEMENT AND A METHOD FOR PREPARATION THEREOF | 2004 |
|
RU2292373C2 |
ACID-SOLUBLE LIGHTWEIGHT PLUGGING MATERIAL TO LIQUIDATE ABSORPTION IN PRODUCTIVE FORMATIONS | 2014 |
|
RU2575489C1 |
METHOD OF PREPARATION OF LIGHT-WEIGHT GROUTING MORTAR | 2002 |
|
RU2215124C1 |
METHOD FOR OBTAINING GEL-FORMING COMPOSITION | 2001 |
|
RU2234598C2 |
Authors
Dates
2004-08-27—Published
2003-02-11—Filed