FIELD: polymer production.
SUBSTANCE: copolymer, prior to supplemented by ingredients, is processed on rolls at 25-45оС for 60-120 min. Then, accelerators, antioxidants, fillers, plasticizers, vulcanization activators, and sulfur are added. Vulcanization is carried out at 141-143оС for 40 min. Vulcanizates can be used for manufacturing hoses, sealing means, and other technical-destination rubber items.
EFFECT: increased frost resistance of vulcanizates.
1 tbl, 16 ex
Title | Year | Author | Number |
---|---|---|---|
BUTADIENE-NITRILE RUBBER BASED RUBBER MIXTURE | 2012 |
|
RU2501820C1 |
RUBBER COMPOUND | 2001 |
|
RU2235741C2 |
BUTADIENE-NITRILE RUBBER BASED COMPOSITION | 2014 |
|
RU2569534C1 |
FROST RESISTANT RUBBER MIXTURE WITH THERMAL EXPANDED GRAPHITE | 2007 |
|
RU2356918C2 |
METHOD OF PREPARING THERMOPLASTIC RUBBER COMPOSITION | 1995 |
|
RU2113445C1 |
METHOD OF EMULSION POLYMERISATION RUBBER STABILISATION | 2007 |
|
RU2373225C2 |
RUBBER COMPOUND | 2001 |
|
RU2235740C2 |
RUBBER MIXTURE MODIFIED WITH COMPOSITION OF ULTRA-HIGH MOLECULAR WEIGHT POLYETHYLENE AND MAGNESIUM NANO-SPINEL | 2010 |
|
RU2425851C1 |
METHOD FOR PRODUCTION OF BUTADIENE-STYRENE(α-METHYL STYRENE) RUBBER BEING MODIFIED BY POLAR MONOMER | 1996 |
|
RU2115664C1 |
METHOD OF PREPARING MOTHER MIXTURE FOR OZONE-RESISTANT BUTADIENE- NITRILE-BASED RUBBER | 1995 |
|
RU2109773C1 |
Authors
Dates
2004-09-10—Published
2002-11-11—Filed