FIELD: electrochemistry.
SUBSTANCE: electrolyte is composed of, in g/l: 50-100 of nickel chloride, 30-45 of boric acid, 2-5 of sodium sulfate, 0.5-2.5 of saccharin, and 4-8 of potassium glycol. The electrolyte allows applying glare nickel coatings for high-density currents from low-concentration electrolyte without mixing and forced pumping of the solution at a temperature of 18-40oC .
EFFECT: enhanced quality of nickel coating.
2 dwg
Title | Year | Author | Number |
---|---|---|---|
LOW-CONCENTRATED ELECTROLYTE FOR BRIGHT NICKEL PLATING | 2002 |
|
RU2213810C1 |
ELECTROLYTE FOR BRIGHT NICKEL PLATING | 0 |
|
SU1737024A1 |
AQUEOUS ELECTROLYTE FOR BRIGHT NICKEL-PLATING, ITS VARIANT | 1993 |
|
RU2071996C1 |
UNSATURATED ISOTHIURONIC SALTS AS COMPONENTS OF ELECTROLYTES FOR BRIGHT NICKEL PLATING | 2014 |
|
RU2559614C1 |
METHOD OF NICKELIZING STEEL, COPPER, AND COPPER ALLOY PARTS | 1996 |
|
RU2089675C1 |
VICTORIA ELECTROLYTE | 1998 |
|
RU2143502C1 |
ELECTROLYTE FOR ELECTROCHEMICAL DEPOSITION OF COATINGS NICKEL-BORON | 2008 |
|
RU2357015C1 |
METHOD FOR ELECTROLYTIC APPLICATION OF PROTECTIVE AND DECORATIVE NICKEL COATINGS ONTO PARTS OF MACHINES AND EQUIPMENT | 2020 |
|
RU2754343C2 |
ELECTROLYTE FOR MIRROR-BRIGHT NICKEL PLATING | 0 |
|
SU1006546A1 |
ELECTROLYTE FOR DIRECT NICKEL-PLATING OF ALUMINIUM AND ITS ALLOYS | 1992 |
|
RU2061104C1 |
Authors
Dates
2005-03-20—Published
2003-12-10—Filed