FIELD: production of fire resistant polyacrylonitrile textile fibers.
SUBSTANCE: claimed method includes continuous thermal treatment of continuous fiber in air media, exothermal heat discharge and pyrolysis product extraction. Continuous tows of 30-40 ktex in thickness with tows of 0.1-0.4 tex in length are heated in four steps: at 150-190°C; at 200-215°C, at 220-240°C, and 250-280°C while fiber draft is 5-30 %. Then fiber is formed to produce crimpiness of 3-7 crimps/cm. Continuous fiber may be cut on sections of 20-125 mm in length.
EFFECT: fire resistant fiber with high strength and elastic characteristics.
3 cl, 6 ex
Title | Year | Author | Number |
---|---|---|---|
TEXTILE YARN FOR MANUFACTURE OF ARTICLES TO BE USED FOR PROTECTING FROM OPEN FIRE | 2004 |
|
RU2286410C2 |
METHOD FOR PRODUCING OF THERMALLY- AND FIRE-RESISTANT TEXTILE MATERIALS | 2006 |
|
RU2310701C1 |
LOW-PILL POLYESTER FIBRE | 2012 |
|
RU2602883C2 |
SINGLE YARN FOR TEXTILE ARTICLES | 2003 |
|
RU2241082C1 |
CARBON TEXTURED THREAD AND METHOD FOR MANUFACTURING THE SAME | 2002 |
|
RU2224057C2 |
COMBINATION YARN | 2015 |
|
RU2620046C1 |
HEAT RESISTANT SEWING THREAD AND METHOD OF ITS MANUFACTURING | 2009 |
|
RU2402649C1 |
HIGH-MODULUS CARBON FIBRE WITH MODIFIED SURFACE FOR REINFORCING COMPOSITES AND METHOD FOR MODIFICATION THEREOF | 2014 |
|
RU2560362C1 |
TECHNICAL FABRIC | 2004 |
|
RU2258105C1 |
POLYACRYLONITRILE CORD OXIDATION METHOD AND APPARATUS | 1999 |
|
RU2167225C1 |
Authors
Dates
2005-08-10—Published
2004-01-15—Filed