FIELD: ceramic compositions.
SUBSTANCE: raw mixture comprises, in mass%, 8.81-9.37 of micro-silicon dioxide, 50.0-53.3 of ash-priming, 3.12-8.6 of carbon lining, 0.06-0.072 of aluminum powder, 0.02-0.31 of sodium carboxymethyl cellulose, and 33.8-35.07 of water. The method comprises preparing the mixture, molding, swelling by vibration, drying at a temperature of 100°C, and roasting at a temperature 800°C.
EFFECT: enhanced strength.
2 cl, 2 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
RAW MATERIAL MIXTURE AND METHOD OF MANUFACTURE OF CERAMIC MATERIALS OF HIGH-POROUS STRUCTURE | 2003 |
|
RU2263088C2 |
RAW MIXTURE AND METHOD FOR PREPARING CERAMIC ARTICLE WITH REDUCED DENSITY | 2001 |
|
RU2206538C1 |
RAW MIXTURE AND METHOD FOR PREPARING CERAMIC MATERIAL WITH REDUCED DENSITY | 2001 |
|
RU2209800C1 |
RAW MIXTURE AND METHOD OF PRODUCTION OF CELLULAR CERAMICS | 2002 |
|
RU2234478C2 |
RAW MIXTURE FOR PRODUCTION OF AIR-ENTRAINED CERAMIC ARTICLES | 2002 |
|
RU2234481C2 |
DRY MIXTURE FOR MAKING CELLULAR FOAMED FIBRE REINFORCED CONCRETE | 2008 |
|
RU2394007C2 |
RAW MIXTURE FOR PREPARING CERAMIC MATERIALS WITH CELLULAR STRUCTURE | 2001 |
|
RU2206549C1 |
RAW MIXTURE AND METHOD FOR MAKING FOAM CERAMIC ARTICLES | 2002 |
|
RU2235699C2 |
RAW MIXTURE AND METHOD OF PRODUCTION OF AIR-ENTRAINED ARTICLES | 2002 |
|
RU2234483C2 |
RAW MIXTURE FOR PREPARING LIGHT TONE ENGOBE FOR WALL CERAMICS | 2008 |
|
RU2378224C1 |
Authors
Dates
2005-10-27—Published
2003-06-03—Filed