FIELD: methods of drying woods.
SUBSTANCE: method can be used at woodworking factories, for example for making furniture. Method of drying is based upon step-by-step change in parameters of drying agent depending on humidity of woods. Timber is preliminary subject to boiling at atmospheric pressure in 15-17% solution of sodium chloride during 2,5-3,0 hours. Then timber is subject to convective drying at four-step increase of temperature from 40° to 60°C and simultaneous four-step reduction of relative humidity of drying agent till achieving value which provides preset final humidity of wood species. Drying agent can have temperature of 40° and relative humidity of 90% at first step, temperature of 50° and relative humidity of 85% at the second step, temperature of 60° and relative humidity of 80% at the third step and temperature of 66° and relative humidity of 50% at the fourth step.
EFFECT: improved quality of drying; reduced time of procedure.
2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
OAK BOGWOOD DRYING TECHNIIQUE | 2007 |
|
RU2350863C1 |
PULSE DRYING METHOD | 2016 |
|
RU2637288C1 |
METHOD OF DRYING OAK BLANKS | 1995 |
|
RU2096702C1 |
TIMBER MATERIAL DRYING METHOD | 1992 |
|
RU2027127C1 |
LUMBER DRYING METHOD | 1991 |
|
RU2030698C1 |
METHOD OF DRYING WOOD | 1992 |
|
RU2045720C1 |
METHOD FOR DRYING OF LUMBER IN CHAMBER DRYING MACHINE OF PERIODIC ACTION | 0 |
|
SU1717916A1 |
WOODWORKING METHOD | 2001 |
|
RU2192348C1 |
METHOD FOR PULSE LUMBER DRYING | 2016 |
|
RU2615854C1 |
METHOD OF CONTROLLING TRIPLE-STAGE DRYING OF WOOD | 0 |
|
SU1539484A1 |
Authors
Dates
2005-10-27—Published
2004-04-19—Filed