FIELD: fur industry, in particular, method for evaluating pickling quality of leather web in tanning of fur and sheepskin raw material.
SUBSTANCE: method involves determining quantitative pickling characteristic of leather web of semi-finished product by using time of solving thereof in alkaline solutions, said time depending on number and kind of intermolecular bindings destructed during pickling. Solving of collagen in alkaline solutions depends upon nature of preliminary acidic preparing procedure. Solving is provided in aqueous solution of potassium hydroxide having concentration of 150 g/l and temperature of 18-20 C. Derma solving time is found after preliminary thermal processing at temperature of 60-65 C during 1.5 hours. Method may be employed both in production of fur and sheepskin products and in fur processing.
EFFECT: wider operational capabilities and reduced time for determining quantitative pickling characteristic of skin web.
1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR DETERMINING PICKLING EXTENT OF LEATHER WEB | 2004 |
|
RU2265215C1 |
METHOD FOR PICKLING OF FUR STOCK | 2009 |
|
RU2399678C1 |
METHOD FOR PICKLING OF SHEEPSKIN-FUR RAW MATERIAL | 2006 |
|
RU2306345C1 |
METHOD FOR PICKLING OF SHIP-FUR STOCK | 2015 |
|
RU2578538C1 |
CORIUM OF GENUINE LEATHER AND FUR SEMIFINISHED PRODUCT AND METHODS FOR MANUFACTURE THEREOF | 2002 |
|
RU2206620C1 |
METHOD OF SEPARATION OF THE DERMIS STRUCTURE OF SHIPSKIN-FUR RAW MATERIAL | 2017 |
|
RU2661852C1 |
METHOD FOR TREATING FUR HIDES | 1988 |
|
SU1556108A1 |
METHOD OF FUR HIDE TREATMENT | 1993 |
|
RU2062791C1 |
METHOD OF PASTE TANNING-STUFFING OF FUR SKINS | 2009 |
|
RU2393234C1 |
FUR SKIN TREATMENT LINE | 1993 |
|
RU2090620C1 |
Authors
Dates
2005-11-27—Published
2004-07-19—Filed