FIELD: disposal of solid waste.
SUBSTANCE: method comprises mixing exhausted mineral oil with granulated slime in the ratio 1:10, adding the mixture obtained to clay to the extent of 20% in mass, roasting the bricks in oxidizing atmosphere at a temperature 960-100° C allowing the bricks to stand at the maximum roasting temperature at least for an hour.
EFFECT: enhanced strength of bricks.
1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
MIXTURE FOR MAKING CERAMIC BRICKS | 2009 |
|
RU2412131C1 |
CERAMIC MIXTURE FOR MAKING LIGHT TONE FACE BRICKS | 2009 |
|
RU2397153C1 |
CERAMIC MASS OF LIGHT TONE FOR FACING BRICK | 2010 |
|
RU2433980C1 |
MIXTURE FOR MAKING CERAMIC BRICK | 2019 |
|
RU2729475C1 |
LIGHT-COLOURED CERAMIC MASS FOR FACE BRICKS | 2023 |
|
RU2810153C1 |
CERAMIC MASS | 1994 |
|
RU2081088C1 |
CERAMIC MASS | 2009 |
|
RU2416585C1 |
MIXTURE FOR MAKING CERAMIC ARTICLES | 2016 |
|
RU2655868C2 |
CERAMIC MASS FOR MANUFACTURING CERAMIC BRICKS | 2023 |
|
RU2798996C1 |
CERAMIC MIXTURE | 2013 |
|
RU2541976C1 |
Authors
Dates
2006-09-10—Published
2005-01-11—Filed