FIELD: manufacture of building materials.
SUBSTANCE: process comprises preparing raw mix, drying molded green brick, and firing it. When preparing raw mix, clay stock with moisture content 18.0-21.0%, activated sludge sediment with total moisture 65%, and additionally ashes obtained upon burning of activated sludge sediment (moisture content 0%) are mixed to form homogeneous process-destined raw mix with density 15.0-21.0%. Ceramic brick manufacture process variations are described.
EFFECT: improved manufacture technology, reduced power consumption, reduced environmental pollution, and improved heat-insulation properties of brick.
6 cl, 3 dwg, 3 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF CERAMIC BRICK | 1993 |
|
RU2082692C1 |
POWER-SAVING METHOD OF PRODUCTION OF THE PORTLAND-CEMENT CLINKER | 2005 |
|
RU2285676C1 |
POWER-SAVING METHOD OF UTILIZATION OF THE CALCIUM SULFATES - THE PHOSPHOGYPSUM AND THE SEDIMENTS OF THE SEWAGE DISPOSAL PLANTS WITH PRODUCTION OF THE CEMENT CLINKER AND THE SULFUR DIOXIDE GAS FOR PRODUCTION OF THE SULFURIC ACID | 2005 |
|
RU2296723C2 |
METHOD OF MANUFACTURING STRUCTURAL, HEAT INSULATING CERAMICS AND COMPOSITION FOR MANUFACTURING THEREOF | 2008 |
|
RU2379258C1 |
RAW MATERIAL MIX FOR MANUFACTURE OF ASH-CERAMIC TILES AND BRICK | 2006 |
|
RU2308439C1 |
METHOD OF MAKING CERAMIC BRICKS | 2015 |
|
RU2611127C2 |
METHOD OF IMPROVEMENT OF CLAY RAW MOLDING AND DRYING PROPERTIES | 2004 |
|
RU2264364C2 |
METHOD OF MAKING WALL CERAMICS | 2015 |
|
RU2593832C1 |
CERAMIC BINDER OF HIGH-PRESSURE STEAM CURING AND METHOD FOR PRODUCTION OF CERAMIC MATERIALS USING THE SAME | 2003 |
|
RU2247696C1 |
METHOD OF MAKING BRICK, BLOCK, FACING PLATE, PLATE FOR INTERNAL WALL FACING | 1994 |
|
RU2085534C1 |
Authors
Dates
2006-09-27—Published
2004-02-17—Filed