FIELD: mechanical engineering.
SUBSTANCE: method comprises dismounting bearing unit, treating the deformed surface by solutions, and applying the repairing agent on the treated surface. The repairing agent is crystallized at a temperature of 70°C and is melted at a temperature above 340°C. The bearing is then heated in oil up to a temperature of 80-90°C, and the bearing unit is assembled.
EFFECT: reduced cost and labor consumption.
Title | Year | Author | Number |
---|---|---|---|
TECHNIQUE OF BABBIT-METAL ALLOYS RECEIVING | 2006 |
|
RU2343216C2 |
METHOD FOR RECLAMATION OF OPEN MINES | 2005 |
|
RU2297533C1 |
TUNNEL-CLEANING HYDRAULIC MECHANICAL COMPLEX | 2010 |
|
RU2421614C1 |
LOOSE MATERIAL CLASSIFIER | 2006 |
|
RU2341338C2 |
METHOD FOR RECULTIVATION OF OPEN-PIT WORKINGS | 2017 |
|
RU2655548C1 |
METHOD OF MANUFACTURE OF STABLE RAILWAY SLEEPER WITH APPLICATION OF MINING AND SMELTING PRODUCTION WASTES | 2007 |
|
RU2335590C1 |
UNDERGROUND MINING WORKINGS VENTILATION METHOD DURING THE ANTICLINAL COAL DEPOSITS COMBINED DEVELOPMENT | 2017 |
|
RU2679015C1 |
AUTOMATED SYSTEM FOR CONTROL AND PREVENTION OF EXPLOSION OF DUST-METHANE-AIR MIXTURE IN COMPLEX MECHANISED MINING FACE | 2010 |
|
RU2459958C1 |
TAPER-RING-GUARD DEVICE TO DEHYDRATE LOOSE MATERIALS | 2007 |
|
RU2361824C2 |
METHOD OF SALVAGING AUTOMOTIVE TIRES AND WASTES OF ORE MINING AND SMELTING | 2008 |
|
RU2406735C2 |
Authors
Dates
2007-04-10—Published
2005-10-24—Filed