FIELD: testing engineering.
SUBSTANCE: method comprises pressing the pyramidal indenter into the cross-section of the coating or material layer until a mark is formed when its diagonals are oriented orthogonal to the direction of residual stress, recording the value of pressure, measuring the area of the mark, and determining the residual stress from the formula proposed.
EFFECT: expanded functional capabilities, reduced labor consumption, and enhanced precision.
1 cl, 5 dwg, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
RESIDUAL STRESS MEASURING METHOD | 1991 |
|
RU2032162C1 |
METHOD OF DETERMINING HARDNESS OF COATING ON ARTICLE | 2018 |
|
RU2698474C1 |
METHOD OF ESTIMATING ABRASIVE WEAR RESISTANCE OF MATERIALS | 0 |
|
SU1786393A1 |
METHOD OF EVALUATION OF DUCTILITY OF HARDENED METAL | 1995 |
|
RU2085902C1 |
METHOD TO DETERMINE SURFACE RESIDUAL STRESSES | 2014 |
|
RU2572670C1 |
METHOD FOR DETERMINING CRYSTALLOGRAPHIC ORIENTATION OF SINGLE CRYSTALS WITH BCC-LATTICE | 0 |
|
SU1000477A1 |
METHOD OF DETERMINING RESISTANCE OF DEFORMATION OF METAL MATERIALS WHEN INDENTING WITH TETRAHEDRAL PYRAMID | 2019 |
|
RU2731034C1 |
MICROHARDNESS ESTIMATION METHOD | 2001 |
|
RU2231040C2 |
METHOD OF MEASURING MICRO-HARDNESS OF TRANSPARENT MATERIALS | 2008 |
|
RU2439533C2 |
METHOD OF KHRUSTALEV E.N. FOR DETERMINING HARDNESS AND STRENGTH PARAMETERS OF MATERIAL MEDIUM | 2016 |
|
RU2615517C1 |
Authors
Dates
2007-11-10—Published
2005-12-21—Filed