FIELD: chemical engineering.
SUBSTANCE: method comprises producing heterogeneous ion exchange film by rolling a mixture of ionite and polymeric binder and supplying the mixture to the calender. The film calendered at a temperature of 125-135°C is provided with reinforcing material and material preventing the film to be glued to the surface of the press.
EFFECT: improved quality of diaphragm.