FIELD: chemistry.
SUBSTANCE: mixture for the given processing contains a 50% water solution of phosphorous-boron-containing methacrylate, neutralised by ammonia to pH 7 and a sodium persulphate initiator in quantity of 1-5% mass of phosphorous-boron-containing methacrylate with the following mass ratios of the components: phosphorous-boron-containing methacrylate - 50.0, water - 50.0, ammonia - 22.0, sodium persulphate - 1.0-5.0.
EFFECT: increased fire-resistance; strength and resistance to thermo-oxidative breakdown.
2 tbl, 3 ex
| Title | Year | Author | Number | 
|---|---|---|---|
| METHOD OF MODIFYING SYNTHETIC FIBRE | 2007 | 
 | RU2330136C1 | 
| COMPOSITION FOR FIRE-PROOF TREATMENT OF POLYETHER FIBRES | 2010 | 
 | RU2435890C1 | 
| COMPOSITION FOR FIRE-PROOF TREATMENT OF SYNTHETIC FIBRES | 2010 | 
 | RU2418897C1 | 
| METHOD OF MODIFYING POLYESTER FIBRE | 2012 | 
 | RU2487205C1 | 
| COMPOSITION FOR FIRE-PROOF TREATMENT OF POLYESTER FIBRES | 2012 | 
 | RU2481428C1 | 
| COMPOSITION FOR FIRE-RESISTANT TREATMENT OF POLYAMIDE FIBRES | 2008 | 
 | RU2378428C1 | 
| COMPOSITION FOR FIRE-PROOF TREATMENT OF POLYAMIDE FIBRES | 2009 | 
 | RU2418898C1 | 
| METHOD FOR MODIFICATION OF POLYAMIDE FIBRES | 2008 | 
 | RU2378427C1 | 
| METHOD FOR MODIFICATION OF POLYAMIDE FIBERS | 2007 | 
 | RU2346095C1 | 
| COMPOSITION FOR FIRE-PROOF TREATMENT OF SYNTHETIC FIBRES | 2010 | 
 | RU2418899C1 | 
Authors
Dates
2008-07-27—Published
2007-03-29—Filed