FIELD: textile industry.
SUBSTANCE: treatment is carried out with composition, which contains the following components in wt parts: 20 borate of methyl phosphite, 1.3 of triethanolamine, 80 of water and 0.20-0.65 of 1% water solution of carboxymethylcellulose at 20°C for 1 min. Fibres are dried on air and thermostatted at 100°C for 30 min.
EFFECT: improved fire-resistance, water-resistance, strength and resistance to thermal-oxidative destruction of polyamide fibres, increased strength of polyamide cord joint to rubber on the basis of chloroprene rubber.
2 tbl, 3 ex
| Title | Year | Author | Number | 
|---|---|---|---|
| COMPOSITION FOR FIRE-RESISTANT TREATMENT OF POLYAMIDE FIBRES | 2008 | 
 | RU2378428C1 | 
| METHOD FOR MODIFICATION OF POLYAMIDE FIBERS | 2007 | 
 | RU2346095C1 | 
| COMPOSITION FOR FIREPROOF PROCESSING OF POLYAMIDE FIBRES | 2007 | 
 | RU2344215C1 | 
| COMPOSITION FOR FIRE-PROOF TREATMENT OF POLYAMIDE FIBRES | 2009 | 
 | RU2418898C1 | 
| COMPOSITION FOR FIRE-PROOF TREATMENT OF SYNTHETIC FIBRES | 2010 | 
 | RU2418899C1 | 
| METHOD OF MODIFYING POLYESTER FIBRE | 2012 | 
 | RU2487205C1 | 
| COMPOSITION FOR FIRE-PROOF TREATMENT OF SYNTHETIC FIBRES | 2010 | 
 | RU2418897C1 | 
| COMPOSITION FOR FIRE-PROOF TREATMENT OF POLYESTER FIBRES | 2012 | 
 | RU2481428C1 | 
| COMPOSITION FOR FIRE-PROOF TREATMENT OF POLYETHER FIBRES | 2010 | 
 | RU2435890C1 | 
| MIXTURE FOR FIRE-PROOF PROCESSING OF SYNTHETIC FIBRES | 2007 | 
 | RU2330135C1 | 
Authors
Dates
2010-01-10—Published
2008-07-21—Filed