FIELD: textile industry.
SUBSTANCE: composition for fire-resistant treatment contains the following components, wt parts: 20 of methyl phosphite borate, 1.3 of triethanolamine, 80 of water and 0.20-0.65 of 1% water solution of carboxymethylcellulose.
EFFECT: increased fire-resistance, water resistance, strength and resistance to thermal-oxidative destruction of polyamide fibres, increased strength of polyamide cord connection to rubber on the basis of chloroprene rubber.
2 tbl, 3 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR MODIFICATION OF POLYAMIDE FIBRES | 2008 |
|
RU2378427C1 |
COMPOSITION FOR FIREPROOF PROCESSING OF POLYAMIDE FIBRES | 2007 |
|
RU2344215C1 |
COMPOSITION FOR FIRE-PROOF TREATMENT OF POLYAMIDE FIBRES | 2009 |
|
RU2418898C1 |
METHOD FOR MODIFICATION OF POLYAMIDE FIBERS | 2007 |
|
RU2346095C1 |
COMPOSITION FOR FIRE-PROOF TREATMENT OF SYNTHETIC FIBRES | 2010 |
|
RU2418899C1 |
COMPOSITION FOR FIRE-PROOF TREATMENT OF SYNTHETIC FIBRES | 2010 |
|
RU2418897C1 |
METHOD OF MODIFYING POLYESTER FIBRE | 2012 |
|
RU2487205C1 |
COMPOSITION FOR FIRE-PROOF TREATMENT OF POLYESTER FIBRES | 2012 |
|
RU2481428C1 |
MIXTURE FOR FIRE-PROOF PROCESSING OF SYNTHETIC FIBRES | 2007 |
|
RU2330135C1 |
COMPOSITION FOR FIRE-PROOF TREATMENT OF POLYETHER FIBRES | 2010 |
|
RU2435890C1 |
Authors
Dates
2010-01-10—Published
2008-07-21—Filed