FIELD: chemistry.
SUBSTANCE: additive to claimed zinc anode mass is an electroconductive fine ceramic powder of titanium nitride (TiN), oxidised in air or pure oxygen medium at 150 to 800°C for a period from 5 minutes to 15 hours before introduction to composition of active zinc anode mass.
EFFECT: significant increase in life span measured in charge-discharge cycle for secondary alkaline electrochemical generator.
8 cl
Title | Year | Author | Number |
---|---|---|---|
NEW SILVER POSITIVE ELECTRODE FOR ALKALINE ACCUMULATOR BATTERIES | 2007 |
|
RU2428768C2 |
ALKALINE SECONDARY ELECTROCHEMICAL GENERATOR WITH ZINC ELECTRODE | 2020 |
|
RU2811938C2 |
DEVICE FOR CATALYTIC GAS RECOMBINATION IN ALKALINE ACCUMULATOR WITH SHORT ZINC ANODE | 2005 |
|
RU2343600C1 |
CATALYTIC AIR CATHODE FOR AIR-METAL BATTERY | 2000 |
|
RU2236067C2 |
METHOD TO PRODUCE NANOSTRUCTURED MULTILAYER 3D COMPOSITE MATERIAL FOR NEGATIVE ELECTRODE OF LITHIUM-ION BATTERY, COMPOSITE MATERIAL, NEGATIVE ELECTRODE AND LITHIUM-ION BATTERY | 2011 |
|
RU2459319C1 |
METAL LITHIUM SUPERDISPERSED DEPOSITED POWDER | 2010 |
|
RU2513987C2 |
POROUS ALUMINUM-WETTING CERAMIC MATERIAL | 2002 |
|
RU2281987C2 |
METHOD FOR CHARGING AIR-ZINC ELEMENT WITH LIMITED CAPACITY | 2013 |
|
RU2615987C2 |
BATTERIES OF BIOMEDICAL DEVICE WITH ELECTRODEPOSITED CATHODES | 2017 |
|
RU2682482C1 |
BATTERIES OF TUBULAR BIOMEDICAL DEVICES WITH CHEMICALLY DEPOSITED SEAL | 2017 |
|
RU2672572C1 |
Authors
Dates
2008-10-10—Published
2003-07-25—Filed