FIELD: textile, paper.
SUBSTANCE: method is referred to bleached wood pulp production from hardwood chips for their further use in different compositions for paper and cardboard production. Chipped wood is impregnated with alkali solution of sodium sulfite. Spent impregnating solution is then removed. Chipped wood is milled in two stages. In between components are treated by alkali solution of hydrogen peroxide at weight concentration 14-18% and final pH=9.5-10.0. Following the second stage of milling, pulp is dissolved to concentration 3.0-5.0% and cured during 30-60 minutes to pH=7.5-8.0. Pulp is chemically treated by alkali solution of hydrogen peroxide between milling stages at 75-85°C during 15-20 minutes.
EFFECT: decrease of chemicals consumption for impregnation and improvement of mechanical and optical properties of target product.
2 cl, 1 tbl, 4 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING BLEACHED CHEMICO-THERMOMECHANICAL WOOD PULP FROM BROAD-LEAVED WOOD | 2003 |
|
RU2230845C1 |
METHOD OF PREPARING WHITENED CHEMICAL-THERMOMECHANICAL MASS FROM LARCH WOOD | 1995 |
|
RU2074919C1 |
METHOD OF PREPARING BLEACHED CHEMICO-THERMOMECHANICAL PULP | 1999 |
|
RU2153545C1 |
METHOD FOR PRODUCING MECHANICAL WOOD PULP | 1996 |
|
RU2106447C1 |
METHOD FOR PRODUCING BLEACHED CHEMICAL, THERMAL AND MECHANICAL PULP FROM LEAF WOOD | 0 |
|
SU1677120A1 |
METHOD OF PRODUCING BLEACHED WOOD PULP | 0 |
|
SU1724763A1 |
METHOD FOR MANUFACTURE OF HIGH-YIELD FIBROUS SEMI-FINISHED PRODUCT | 2003 |
|
RU2233927C1 |
METHOD OF PRODUCING THERMOCHEMICALLY TREATED PULP | 0 |
|
SU1721148A1 |
METHOD FOR PRODUCTION OF FIBROUS SEMI-PRODUCT OF MISCANTHUS | 2019 |
|
RU2736428C1 |
METHOD OF PRODUCING WOODEN PULP | 0 |
|
SU979554A1 |
Authors
Dates
2008-10-20—Published
2007-01-17—Filed