FIELD: paper-and-pulp industry.
SUBSTANCE: wood pulp is steamed at 105-120оС, treated with hydrogen peroxide, sodium peroxide, and complexing agent. Simultaneously, first step of grinding is carried out followed by second-step grinding and bleaching. Bleached pulp is subjected to further grinding at pulp concentration 2-5% and degree of grinding exceeding degree of the second-step grinding by a specified value. Treatment of steamed wood may be performed in presence of sodium silicate. Broad-leaved wood is selected from birch, aspen wood, and mixture thereof.
EFFECT: increased yield of desired product and increased its mechanical strength.
4 cl, 1 tbl, 7 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING WHITENED CHEMICAL-THERMOMECHANICAL MASS FROM LARCH WOOD | 1995 |
|
RU2074919C1 |
METHOD OF PREPARING BLEACHED CHEMICO-THERMOMECHANICAL PULP | 1999 |
|
RU2153545C1 |
METHOD FOR PRODUCING BLEACHED CHEMICAL, THERMAL AND MECHANICAL PULP FROM LEAF WOOD | 0 |
|
SU1677120A1 |
METHOD FOR PRODUCING MECHANICAL WOOD PULP | 1996 |
|
RU2106447C1 |
COMPOSITION FOR MANUFACTURING HEAT-SENSITIVE PAPER | 2016 |
|
RU2642801C1 |
METHOD OF WOOD PULP PRODUCTION | 2007 |
|
RU2336383C1 |
METHOD FOR PRODUCING EXTRUSIVE THERMOMECHANICAL MASS | 2021 |
|
RU2780995C1 |
METHOD OF PRODUCING BLEACHED WOOD PULP | 0 |
|
SU1724763A1 |
WOOD-PULP BLEACHING PROCESS | 2000 |
|
RU2155834C1 |
METHOD FOR MANUFACTURING HIGH-OUTPUT FIBROUS SEMI-FINISHED PRODUCT | 2004 |
|
RU2281353C1 |
Authors
Dates
2004-06-20—Published
2003-04-17—Filed