FIELD: construction.
SUBSTANCE: method of decorative filling aggregate manufacturing includes application on aggregate particles surface at least one layer of cement paste with its further consolidation, impregnation of aggregate particles with consolidated layer by sodium ethyl-siliconate or methyl-siliconate with its further drying at temperature 20-25°C during 24 hours.
EFFECT: absorption of water reduction.
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR MANUFACTURING DECORATIVE FILLER | 2007 |
|
RU2334711C1 |
METHOD OF PRODUCTION OF DECORATIVE AGGREGATE | 2007 |
|
RU2320599C1 |
METHOD FOR MANUFACTURING AGGREGATE FOR CONCRETE | 2007 |
|
RU2331600C1 |
METHOD FOR MANUFACTURING COARSE AGGREGATE FOR CONCRETE | 2007 |
|
RU2334712C1 |
METHOD OF PRODUCING POROUS AGGREGATE | 2013 |
|
RU2538026C1 |
METHOD FOR MAKING CONCRETE ARTICLES HAVING PROTECTIVE-DECORATIVE COATING | 2006 |
|
RU2302335C1 |
METHOD OF PRODUCTION OF LARGE-SIZE FILLER FOR CONCRETE | 2008 |
|
RU2377205C1 |
METHOD FOR MANUFACTURING OF COARSE FILLER FOR CONCRETES | 2008 |
|
RU2372304C1 |
METHOD OF PRODUCING COARSE AGGREGATE FOR CONCRETE | 2012 |
|
RU2481287C1 |
RAW MATERIAL MIXTURE FOR MANUFACTURING OF COARSE AGGREGATE ENVELOPE | 2012 |
|
RU2508275C1 |
Authors
Dates
2008-10-27—Published
2007-02-14—Filed