FIELD: metallurgy.
SUBSTANCE: investment contains, wt %: 9.99-72.80 of quartz-bearing component with containing of SiO2 not less than 96 wt % and grain size 0.1-1.0 mm; 14.98-77.67 chromite concentrate and/or chromite ore with content of Cr2O3 not less than 35 wt % and grain size 0.1-1.0 mm; 0.05-9.70 of graphite with grain size less than 0.1 mm; 0.01-2.91 olein and/or stearic acid.
EFFECT: fluidity increasing of investment, density increasing of its stowage into free poured condition, hardening againstk iron-containing melts, probability reduction of mixture sintering ability.
2 tbl
Title | Year | Author | Number |
---|---|---|---|
INVESTMENT FOR FILLING UP OF LADLE CHANNEL | 2008 |
|
RU2381088C1 |
COMPOSITE STARTING MIXTURE FOR FILLING THE STEEL-TEEMING LADLE DISCHARGE CHANNEL | 2018 |
|
RU2696609C1 |
MIXTURE FOR FILLING DISCHARGING DUCT OF STEEL CASTING LADLE | 2006 |
|
RU2302319C1 |
METHOD OF FILLING WITH REFRACTORY MATERIAL OUTLET CHANNEL OF STEEL CASTING LADLE | 2019 |
|
RU2712206C1 |
MIXTURE FOR FILLING OUTLET DUCT OF STEEL CASTING LADLE | 2006 |
|
RU2302318C1 |
RAW MIXTURE FOR PREPARING CLINKER | 0 |
|
SU927782A1 |
CHROMITE-PERICLASE REFRACTORY | 2022 |
|
RU2785728C1 |
FIREPROOF MIXTURE FOR FILLING OF LADLE STEEL EXHAUST CHANNEL | 2004 |
|
RU2242441C1 |
FACING MATERIAL FOR MOULDS AND CORES | 2011 |
|
RU2450885C1 |
CARBON OXIDE REFRACTORY MATERIAL | 2007 |
|
RU2356869C1 |
Authors
Dates
2009-02-10—Published
2006-11-02—Filed