FIELD: metallurgy.
SUBSTANCE: belit is received by mixing and sintering at the temperature 1250-1420°C of material, containing no less than 10% SiO2 and no less than 2.5% Al2O3 and limestone component. Received material is quenched from the sintering temperature till 201-216°C and isolated in this temperature interval during the time, necessary for formation of ceiling amount of β-Ca2SiO4.
EFFECT: reduction of forming temperature of belit.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
PRODUCTION OF ALUMINIUM-BEARING CAKE | 2012 |
|
RU2521577C2 |
METHOD OF ALUMINIUM-CONTAINING SINTER PRODUCTION | 2008 |
|
RU2364572C1 |
METHOD OF PROCESSING ALKALINE ALUMINOSILICATE MATERIAL | 2023 |
|
RU2819963C1 |
METHOD OF PROCESSING NEPHELINE ORES AND CONCENTRATES | 2007 |
|
RU2340559C1 |
CHARGE FOR ALUMINA PRODUCTION | 2006 |
|
RU2327642C1 |
PRODUCTION OF CEMENT CLINKER | 2012 |
|
RU2555980C2 |
MAGNESIA SPINEL-BASED FUSED MATERIAL AND METHOD OF PRODUCING SAID MATERIAL | 2009 |
|
RU2417201C2 |
METHOD OF PROCESSING ALUMINUM-CONTAINING RAW MATERIAL | 2006 |
|
RU2313491C1 |
METHOD FOR OBTAINING CALCIUM ALUMINOSILICATE INORGANIC COAGULANT | 2018 |
|
RU2683082C1 |
METHOD OF CONVERSION OF BAUXITES INTO ALUMINA | 2003 |
|
RU2232716C1 |
Authors
Dates
2009-04-20—Published
2006-10-18—Filed