FIELD: metallurgy.
SUBSTANCE: electrolyte contains six-water nickel chloride 200-350 g/l, boric acid 25-40 g/l, saccharine 0.7-1.8 g/l, aluminium oxide 15-40 g/l, deca-hydro-decaborate of sodium 1.2-4.5 g/l.
EFFECT: increased micro-hardness.
2 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
GALVANIC COMPOSITE MATERIAL ON BASE OF NICKEL | 2009 |
|
RU2422561C2 |
ELECTROLYTE FOR SEDIMENTATION OF COMPOSITION COATING NICKEL-COBALT-DIAMOND | 2008 |
|
RU2362843C1 |
NICKEL-BASED GALVANIC COMPOSITE MATERIAL | 2008 |
|
RU2360044C1 |
PROCEDURE FOR PRODUCTION OF COMPOSITE ELECTRO-PLATE NICKEL-COBALT-ALUMINIUM OXIDE AND COMPOSITE ELECTRO-PLATE NICKEL-COBALT- ALUMINIUM OXIDE | 2009 |
|
RU2418107C2 |
ELECTROLYTE TO DEPOSIT COMPOSITE COATING OF ZINC AND FLUOROPLASTIC | 2011 |
|
RU2464363C1 |
COMPOSITION ELECTROCHEMICAL PLATING | 1992 |
|
RU2048573C1 |
COMPOSITION NICKEL COBALT FTOROPLASTIC COATING ELECTROLYTE | 2008 |
|
RU2352694C1 |
ELECTROLYTE FOR DEPOSITION OF NICKEL-COBALT-SILICON OXIDE-PLASTIC FLUOR COMPOSITE COATING | 2012 |
|
RU2489530C1 |
ELECTROLYTE FOR ELECTROCHEMICAL DEPOSITION OF COATINGS NICKEL-BORON | 2008 |
|
RU2357015C1 |
GALVANIC NICKEL COMPOSITE | 2008 |
|
RU2352693C1 |
Authors
Dates
2011-05-10—Published
2009-03-12—Filed