FIELD: electricity.
SUBSTANCE: electrolyte contains zinc sulfate 200 - 250 g/l, aluminium sulfate 20 - 30 g/l, sodium sulfate 50 - 100 g/l, dextrin 8 - 10 g/l and a fluoroplastic suspension 0.3 - 0.9 ml/l.
EFFECT: application of a proposed electrolyte makes it possible to apply a composite coating of zinc and fluoroplastic, which has higher corrosion resistance.
2 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
ELECTROLYTE FOR DEPOSITING COATING OF TIN-ZINC ALLOY BASED COMPOSITE MATERIAL | 2012 |
|
RU2493296C1 |
GALVANIC COMPOSITE MATERIAL BASED ON STANNUM-ZINC ALLOY | 2012 |
|
RU2489528C1 |
ELECTROLYTE FOR DEPOSITION OF COMPOSITE COATS BASED ON NICKEL | 1995 |
|
RU2089678C1 |
ELECTROLYTE SUSPENSION FOR FORMATION OF NICKEL-FLUOROPLASTIC COATINGS | 1999 |
|
RU2155246C1 |
METHOD OF OBTAINING COMPOSITE ELECTROCHEMICAL COATING ON STEEL | 2015 |
|
RU2618679C1 |
ANTIFRICTION COATING OF COPPER-FLUOROPLASTIC | 2017 |
|
RU2696376C2 |
VICTORIA ELECTROLYTE | 1998 |
|
RU2143502C1 |
ELECTROLYTE FOR PRECIPITATION OF ALLOY ZINC-BORON | 0 |
|
SU1650785A1 |
METHOD OF PRODUCING ZINC-NANODIAMOND ELECTROCHEMICAL COATING | 2016 |
|
RU2689355C1 |
ELECTROLYTE FOR DEPOSITION OF NICKEL-BORON-FLUOROPLASTIC COMPOSITE MATERIAL | 2002 |
|
RU2213812C1 |
Authors
Dates
2012-10-20—Published
2011-04-04—Filed