FIELD: chemistry.
SUBSTANCE: invention relates to compositions for hot repairing of fireproof masonry of industrial furnaces by method of ceramic welding and can be used in metallurgical industry in coke chemical production. Ceramic mixture for repairing coke furnace masonry includes quartz sand, silicon and coke dust with the following component ratio in wt %: quartz sand - 65-75; silicon -15 -30; coke dust -5-15.
EFFECT: obtaining heat-resistant and mechanically durable ceramic welding with homogeneous mineralogical composition.
3 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
CERAMIC SURFACING MIXTURE | 2005 |
|
RU2290384C2 |
POWDERED MIXTURE FOR CUTTING REFRACTORY (VERSIONS) | 2010 |
|
RU2434829C1 |
MIXTURE FOR THE WELDING SURFACING AND WELDING TOGETHER OF CHAMOTTE AND SILICA AND THE METHOD OF THE MIXTURE APPLICATION | 2005 |
|
RU2299870C2 |
MIXTURE FOR FUSING AND WELDING CHAMOTTE AND DINAS | 1996 |
|
RU2096387C1 |
BLEND FOR CERAMIC WELD DEPOSITION ONTO FIRECLAY BRICKWORK | 1993 |
|
RU2074152C1 |
EXOTHERMIC REFRACTORY MORTAR | 1996 |
|
RU2163579C2 |
METHOD OF CERAMIC SURFACING AND DEVICE FOR REALIZATION OF THIS METHOD | 2005 |
|
RU2291201C1 |
METHOD FOR REPAIRING REFRACTORY LINING OF HEARTH OF HEAT AGGREGATES BY CERAMIC FUSION AND TERMITE REFRACTORY MASS FOR CERAMIC FUSION | 1999 |
|
RU2158403C1 |
METHOD OF POWDER CUTTING OF REFRACTORY MATERIAL AND DEVICE TO THIS END | 2010 |
|
RU2434744C2 |
FIREPROOF MATERIAL FOR MOUNTING AND REPAIR OF BRICK-LINING OF THERMAL UNITS | 2012 |
|
RU2497779C1 |
Authors
Dates
2009-04-27—Published
2007-07-17—Filed