FIELD: chemistry; metallurgy.
SUBSTANCE: ceramic substrate is placed on melted lead or eutectic Pb-Bi surface with dissolved deposited metal. Then the ceramic substrate surface is cooled to ensure temperature gradient 600-700°C between the melt and its surface. Further it is kept in the inert gas medium until nanostructured metal plate of the required thickness is deposited on the ceramic substrate surface. Thereafter the plate is removed from the substrate.
EFFECT: improved durability.
5 cl, 1 dwg, 3 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF NANOSTRUCTURED METAL LAYER FORMATION ON STEEL PLATE SURFACE | 2007 |
|
RU2354750C1 |
METHOD FOR CHEMICAL AND HEAT TREATMENT OF STEEL PRODUCTS | 0 |
|
SU954502A1 |
METHOD AND DEVICE FOR PREPARING CYCLOTRON TARGETS AND RADIOACTIVE RADIATION SOURCES | 2006 |
|
RU2310249C1 |
METHOD FOR PRODUCING METAL COATINGS | 0 |
|
SU1016397A1 |
VACUUM PROCESS UNIT FOR MAKING NANOSTRUCTURED COATS WITH SHAPE MEMORY EFFECT ON PART SURFACE | 2014 |
|
RU2563910C1 |
METHOD OF PROCESSING LEAD-ZINC WASTES CONTAINING TIN AND COPPER | 1997 |
|
RU2130501C1 |
NUCLEAR POWER PLANT WITH CERAMIC FAST NEUTRON REACTOR | 2021 |
|
RU2755261C1 |
METHOD OF OBTAINING DIFFUSION MULTIPLE-INGREDIENT PROTECTIVE COATINGS | 0 |
|
SU644869A1 |
THIN-FILM NANOSTRUCTURED ELECTRODE MATERIAL AND METHOD OF PRODUCING SAID MATERIAL | 2009 |
|
RU2414771C1 |
CONVERTER OF HIGH-ENERGY PARTICLES AND MODE OF PRODUCTION OF A FILM | 2005 |
|
RU2302015C2 |
Authors
Dates
2009-05-10—Published
2007-07-02—Filed