FIELD: chemistry.
SUBSTANCE: invention concerns method of obtaining polyurethanedi(met)acrylates applicable as binders for powder coatings applied on metal substrates, plastic parts, fiber-reinforced plastic parts. Polyurethanedi(met)acrylates are obtained by interaction of diisocyanate component, diol component and hydroxy-C2-C4-alkyl(met)acrylate at mol ratio of x:(x-1):2, where x takes any value from 2 to 5. 1,6-hexanediisocyanate comprises 50 to 80 mol % of diisocyanate component, and one or two diisocyanates selected out of defined diisocyanate group where mol content of respective diisocyanates amount to 100 mol % comprise(s) 20 to 50 mol %, so that each diisocyanate comprises at least 10 mol % of diisocyanate component. Diol component includes not more than four different diols, and at least one linear aliphatic alpha, omega-C2-C12-diol comprises 20 to 100 mol % of diol component, while at least one (cyclo)aliphatic diol different from linear aliphatic alpha, omega-C2-C12-diols comprises 0 to 80 mol %. Each diol of the diol component comprises at least 10 mol % of diol component, and mol content or respective diols amounts to 100 mol %. Due to the absence of solvent in polyurethanedi(met)acrylate production, further cleaning of end product is not required, thus increasing process product output.
EFFECT: higher acid resistance of coating films applied and solidified with the use of powder coatings containing claimed polyurethanedi(met)acrylates.
6 cl, 15 ex, 3 tbl
Authors
Dates
2009-05-20—Published
2005-10-13—Filed