SUBSTANCE: in method of thermal treatment of welded joints of volume tempered rails in content of travelling rail-welding machine on the way it is heated rail section in area of joint weld up to 850-900°C and forcecooled head with simultaneous cooling of neck and bottom normally on air. At thermal treatment of welded joints of rails in content of travelling rail-welding machines on the way for metal strengthening of welded joint of head of rails it is applied air flow with pressure 0.5-0.8 MPa and consumption 0.08-0.15 m3/d. Air is fed during not less than 180 s at a rate 60-200 m/s on surface of rail through row of openings of diametre 2 mm each and with total area 0.0008-0.0011 m2, located in plane panel of bottom part of quench with air collector of volume 0.002-0.003 m3. Air collector is installed at a distance not more than 10 mm between surface of rail head and plane lower the panel with openings.
EFFECT: method provides required solidity of metal, persistence and wear resistance of joints of volume tempered rails, welded in content of travelling, rail-welding machines on the way.
Title | Year | Author | Number |
---|---|---|---|
METHOD OF HEAT TREATMENT OF RAIL WELD JOINTS | 2012 |
|
RU2524526C1 |
METHOD OF CONTACT BUTT WELDING OF RAILS | 2020 |
|
RU2743440C1 |
METHOD OF HEAT TREATMENT OF RAIL WELDED JOINTS | 2006 |
|
RU2309185C1 |
METHOD OF CONTACT BUTT WELDING OF RAILS | 2016 |
|
RU2641586C1 |
INSTALLATION FOR THERMAL PROCESSING OF WELDED JOINTS OF RAILS | 2018 |
|
RU2704951C1 |
METHOD OF MANUFACTURING RAIL LASHES AND COMPLEX FOR IMPLEMENTING METHOD | 2017 |
|
RU2681046C1 |
METHOD AND DEVICE FOR THERMAL PROCESSING OF WELDED RAIL CONNECTIONS | 2017 |
|
RU2667574C1 |
METHOD OF THERMALLY TREATING WELDED RAILS | 0 |
|
SU1735392A1 |
METHOD FOR QUALITY CONTROL OF WELDED JOINT OF RAIL JOINT | 2018 |
|
RU2698508C1 |
METHOD FOR INDUCTIVE THERMAL HARDENING OF SWITCH RAILS AND INSTALLATION FOR ITS IMPLEMENTATION | 2022 |
|
RU2794329C1 |
Authors
Dates
2009-10-27—Published
2008-04-29—Filed