FIELD: transportation.
SUBSTANCE: after preliminary machining, heating the rail ends to be welded and settling are carried out. After settling, an exposure of 5÷15 seconds is carried out, then alternating electric current 2÷4 is passed through the welded joint in pulses with the duration of 0.5÷220 seconds at the intervals of 10÷40 seconds at the current density of 2÷40 A/mm2.
EFFECT: required microstructure and mechanical properties of the welded joint without additional heat treatment, excluding the defects in the weld seam and the weld zone, reducing the duration of the rail joining process.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF CONTACT BUTT WELDING OF RAILS | 2020 |
|
RU2743440C1 |
METHOD OF CONTACT BUTT WELDING OF RAILS | 2019 |
|
RU2725821C1 |
RESISTANCE BUTT WELDING MACHINE | 2017 |
|
RU2683668C1 |
METHOD FOR CONTACT BUTT WELDING OF RAILS | 2021 |
|
RU2756553C1 |
METHOD FOR OPTIMIZING THE MODES OF CONTACT WELDING OF RAILS | 2022 |
|
RU2792955C1 |
METHOD FOR CONTACT FLASH-BUTT WELDING OF CAST IRON | 2003 |
|
RU2240904C1 |
METHOD FOR CONTACT FLASH WELDING | 2017 |
|
RU2644484C1 |
METHOD OF RESISTANCE FUSION WELDING OF STEEL RAILS | 2005 |
|
RU2296655C2 |
METHOD OF RELIEF WELDING OF RAILS | 2022 |
|
RU2809616C1 |
CONTROL OVER WELDING OF PIPELINES FROM HIGH-STRENGTH PIPES WITH CONTROLLED HEAT INPUT | 2014 |
|
RU2563793C1 |
Authors
Dates
2018-01-18—Published
2016-12-07—Filed