FIELD: production processes.
SUBSTANCE: invention refers to abrasive treatment and can be used during manufacture of rubber wheels, and namely cutter wheels. Wheel workpiece is heated up to maximum heating temperature during 1.5÷2.0 hours, exposed at this temperature during 4.0÷4.5 hours, and then cooled to 120÷125°C and exposed at this temperature for 1.0÷1.5 hours.
EFFECT: improving wheel hardness and decreasing allowance for mechanical treatment with a view to increase of steadiness of workpiece geometrical shape during its vulcanisation.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR MAKING VULCANITE-BINDER CUT-OFF ABRASIVE WHEELS | 2002 |
|
RU2227775C2 |
MASS FOR PRODUCING ABRASIVE TOOL | 2009 |
|
RU2413603C1 |
PROCESS TESTING PROPERTIES OF RUBBER-CARRYING MIXTURES | 1997 |
|
RU2127426C1 |
PASTE FOR MANUFACTURING ABRASIVE TOOLS | 2004 |
|
RU2269408C2 |
MASS FOR MAKING ABRASIVE TOOL | 2001 |
|
RU2200082C2 |
METHOD AND DEVICE FOR PRODUCING ABRASIVE TOOL WITH VULCANITE BINDER | 1996 |
|
RU2104145C1 |
METHOD OF MAKING ABRASIVE TOOL ON VULCANITE BINDER | 1997 |
|
RU2126740C1 |
COMPOSITION FOR MAKING POLISHING ABRASIVE ELASTIC WHEELS | 2005 |
|
RU2311280C2 |
METHOD OF PRODUCTION OF ABRASIVE WHEEL BLANKS ON VULCANITE BINDER AND DIE FOR ITS REALIZATION | 1997 |
|
RU2108228C1 |
UNIVERSAL SHEARING DIE | 2000 |
|
RU2174905C1 |
Authors
Dates
2009-12-20—Published
2008-09-02—Filed