FIELD: construction.
SUBSTANCE: method includes production of alkali activated hydraulic binder containing slag and amino silicates where slag is represented as an ingredient in the amount from 20% wt. Aluminosilicates different from aluminium smelting is represented in the amount from 5 to 75% wt, and alkali activating agent in the amount corresponding to the equivalent to Na2O identified as (Na2O + 0.658 K2O) (ASTM C 150) between 0.7 and 4% wt, correspondingly, relative to all mixture content. As disclosed by the invention, the method also includes mixture treatment at temperatures below 50°C during 4-6 hours. Invention is disclosed in dependent points.
EFFECT: increased early and final strength, reduced water-cement ratio and increased crack strength.
9 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
BINDER BASED ON CALCIUM ALUMINO-SILICATE DERIVATIVES FOR CONSTRUCTION MATERIALS | 2017 |
|
RU2715583C1 |
CONSTRUCTION MIXTURE BASED ON SLAG ACTIVATED BY SIDE PRODUCT | 2018 |
|
RU2768568C2 |
CINDER BINDER | 2010 |
|
RU2448063C2 |
BINDER BASED ON SOLID MINERAL COMPOUND RICH IN ALKALI-EARTH METAL OXIDE WITH PHOSPHATE-CONTAINING ACTIVATORS | 2015 |
|
RU2698790C2 |
CONTROL OF SETTING TIME OF GEOPOLYMER COMPOSITIONS CONTAINING REACTIVE ALUMINOSILICATE MATERIALS CHARACTERIZED BY HIGH CA CONTENT | 2018 |
|
RU2795134C2 |
METHOD FOR OBTAINING A LOW-CLINKER HYDRAULIC BINDER BASED ON METALLURGICAL SLAGS FOR THE MANUFACTURE OF FILLING MIXTURES | 2020 |
|
RU2753802C1 |
BRIQUETS FOR MANUFACTURING MINERAL WOOL, METHODS FOR MANUFACTURING BRIQUETS AND MINERAL WOOL | 1991 |
|
RU2090525C1 |
HYDRAULIC BINDING AGENT BASED ON SULFO-ALUMINOUS CLINKER AND PORTLAND CEMENT CLINKER | 2009 |
|
RU2513572C2 |
COLORFAST JOINTING MATERIALS | 2001 |
|
RU2264362C2 |
BINDING AGENT | 1997 |
|
RU2125545C1 |
Authors
Dates
2009-12-20—Published
2005-04-05—Filed