FIELD: chemistry.
SUBSTANCE: invention relates to spheroidal particles of polyester polymer and products made from the said particles. The particles are characterised by inherent viscosity It.V of at least 0.72 dl/g and/or at least two pressure peaks, and/or low degree of crystallinity in an interval of at least 20% and maximum degree of crystallinity Tcmax, and optionally but preferably contain 10 parts/million or less residual acetaldehyde. The spheroidal particles are dried, molten and objects are moulded from the molten mass.
EFFECT: provision for minimal degree of aggregation of particles in the drier.
43 cl, 5 dwg, 5 tbl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
REMOVAL OF RESIDUAL ACETALDEHYDE FROM POLYESTER PARTICLES | 2005 |
|
RU2388767C2 |
POLYESTER PARTICLES HAVING SMALL MOLECULAR MASS GRADIENT FROM SURFACE TO CENTRE | 2005 |
|
RU2384590C2 |
HIGH-MOLECULAR WEIGHT POLYMER ESTERS CHARACTERISED BY LOW CONTENT OF ACETALDEHYDE | 2008 |
|
RU2474592C2 |
LOW-MELTING POLYESTER POLYMERS | 2005 |
|
RU2388605C2 |
SECTIONED POLYMER TABLETS | 2005 |
|
RU2370365C2 |
POLYESTER POLYMERS WITH LOW RATE OF FORMATION OF ACETALDEHYDE AND HIGH CONCENTRATION OF TERMINAL VINYL GROUPS | 2008 |
|
RU2458074C2 |
POLYESTERS CONTAINING ALUMINIUM/ALKALI METAL OR ALKALI/TITANIUM, HAVING HIGH REHEATING CAPACITY, IMPROVED COLOUR AND TRANSPARENCY | 2006 |
|
RU2434900C2 |
ALUMINIUM-CONTAINING POLYESTER POLYMERS, HAVING LOW RATE OF FORMATION OF ACETALDEHYDE | 2006 |
|
RU2448124C2 |
POLYMERS BASED ON POLYESTERS HAVING HIGH INTRINSIC VISCOSITY OF MOLTEN PHASE WITH SUITABLE RATE OF FORMATION OF ACETALDEHYDE | 2006 |
|
RU2402575C2 |
PROCEDURE FOR INTRODUCTION OF ADDITIVES INTO POLYMER MELT | 2006 |
|
RU2418010C2 |
Authors
Dates
2010-04-20—Published
2005-08-29—Filed