FIELD: machine building.
SUBSTANCE: here is disclosed procedure for production of poly-ethylene-terephtalate items by means of drawing polymer item of stretched shape in adsorption-active fluid medium containing dissolved silver salt, and by means of drying item in isometric conditions with successive heat treatment of item at 50°C and above during not less, than 5 sec. Film, fibre, tube, rod or tape can be used as a polymer item of stretched shape.
EFFECT: simplified production of poly-ethylene-terephtalate items and raised antibacterial properties compared to known.
6 cl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING POLYMER ARTICLES WITH ANTIBACTERIAL PROPERTIES BASED ON SEMI-CRYSTALLINE POLYMERS | 2019 |
|
RU2717268C1 |
METHOD OF PRODUCING METAL-POLYMER NANOCOMPOSITE MATERIALS WITH METAL NANOPARTICLES | 2018 |
|
RU2711427C1 |
METHOD OF INTRODUCING ADDITIVES INTO POLYMERS | 2008 |
|
RU2370506C1 |
METHOD OF INTRODUCING ADDITIVES INTO POLYMERS | 2008 |
|
RU2375176C1 |
METHOD OF INTRODUCING ADDITIVES INTO POLYMERS | 2008 |
|
RU2370507C1 |
METHOD OF RECORDING INFORMATION ON POLYMERS | 2007 |
|
RU2361886C1 |
METHOD OF MAKING POLYMER-BASED TEMPERATURE SENSORS | 2007 |
|
RU2387750C2 |
METHOD OF INTRODUCING ADDITIVES INTO POLYMER | 2014 |
|
RU2585001C2 |
METHOD OF INTRODUCING ADDITIVES INTO POLYMER | 2014 |
|
RU2585003C2 |
METHOD FOR OBTAINING NANOPOROUS POLYMER MATERIALS | 2014 |
|
RU2576049C2 |
Authors
Dates
2010-07-20—Published
2008-07-01—Filed