FIELD: chemistry.
SUBSTANCE: invention can be particularly used in the cable industry when making electrical cable shielding used in explosive environments, in electrical engineering when making working sheath of earthing electrodes in general-purpose protective earthing systems, protection from static electricity and electrochemical protection from corrosion in the ground, fresh and sea water etc. The rubber mixture contains the following in pts. wt: synthetic ethylenepropylene diene rubber 90-100, technical sulphur 0.3-0.5, paraffin-naphthalene oil 10-15, bis-tertbutylperoxyisopropyl benzene 5.0-6.5, zinc oxide 5-8, electroconductive technical carbon 80-100, carbon-fibre material made from hydrocellulose fibre 15-25. The electrical current conductor comprises at least one conductor which has a shielding or working sheath made from the said rubber mixture.
EFFECT: improved operational characteristics of the electroconductive rubber mixture and electrical current conductors made from the said mixture.
4 cl, 2 tbl, 3 ex
Title | Year | Author | Number |
---|---|---|---|
ELECTRICALLY CONDUCTIVE RUBBER COMPOSITION FOR SOLID TIRES AND DOES NOT LEAVE TRACE SOLID TIRE | 2019 |
|
RU2731635C1 |
FIREPROOF RUBBER MIXTURE | 2012 |
|
RU2522627C2 |
RUBBER COMPOSITION AND BASED ON IT GOODS AND THEIR METHOD OF PRODUCTION | 2007 |
|
RU2358627C2 |
FIRE RESISTANT RUBBER COMPOUND | 2018 |
|
RU2746216C2 |
FIREPROOF RUBBER MIXTURE | 2014 |
|
RU2567292C1 |
FROST AND OIL-RESISTANT RUBBER MIXTURE BASED ON CAOUTCHOUC MIXTURES AND A METHOD FOR PRODUCTION THEREOF | 2019 |
|
RU2705069C1 |
RUBBER COMPOUND (VERSIONS) | 1997 |
|
RU2149165C1 |
FROST-RESISTANT RUBBER MIXTURE FOR MANUFACTURE OF RUBBER PRODUCTS WITH WIDE OPERATING TEMPERATURE RANGE | 2023 |
|
RU2807833C1 |
WATER-OIL-SWELLING THERMOPLASTIC ELASTOMER COMPOSITION | 2018 |
|
RU2690929C1 |
RUBBER MIX FOR PRODUCTION OF WATERPROOF MATERIALS (VERSIONS) | 2004 |
|
RU2277108C1 |
Authors
Dates
2010-09-10—Published
2008-10-02—Filed